Figure 8 (a) Schematic rendering of the in situ additive manufacturing setup implemented at BL3W1 of Beijing Synchrotron Radiation Facility. (b) The 9 kHz time-resolved diffraction patterns of Ti alloy during a laser melting of 1 ms. |
|